A custom lead frame for IC packaging can be made two ways: photo-etched or stamped. Both are real processes, both ship in volume, and the wrong choice costs a buyer in one of two places — either a die that has to be re-cut every time the design moves, or a pattern too fine for the process chosen. The question this post answers is the one a packaging engineer asks before the drawing is released: for this lead frame, at this pitch, this volume and this stage of the design, which process should it be?
The short answer is that etching wins when the pattern is fine, the volume is low or uncertain, or the design is still moving — and stamping wins when the design is frozen, the pattern is simple, and the volume is large enough for a hard die to pay for itself. The rest of this post works that answer into numbers a buyer can check against a drawing: the tolerance rule, the thickness rule, the half-etch capability, and the four things a lead-frame drawing must carry.
Answer capsule: six things a buyer needs
- A lead frame is the metal skeleton of an IC package. A die pad that carries the chip, inner leads bonded to the die, outer leads soldered to the board, and tie bars that hold the strip together until singulation. It is used in QFN, QFP, SOP and DIP-style packages.
- Etching wins on fine pitch, because there is no die to hold the pattern. Through-features floor at roughly 0.8–1.2× the material thickness: on 0.1 mm stock a gap floors near 0.08–0.12 mm; on 0.2 mm stock, near 0.16–0.24 mm. The lead width itself carries the ±10% tolerance rule.
- Etching wins on revisions, because the tooling is digital. A design change is a new film, not a re-cut die. Samples in 3–5 days, prototype-to-production on the same tooling, no minimum order — a pilot lot can be etched without a die investment.
- Etching wins on features stamping cannot do in one pass. Half-etch steps, grooves and recesses at 50–75% of thickness, depth controlled to ±0.05 mm — a die pad stepped down from the lead plane, or a thinned section, in the same etch as the through-pattern.
- Stamping wins on a frozen, high-volume, simple design. A hard die spreads its cost over a very large, stable run. Etching does not pretend otherwise — the decision is about volume and design stability, not about one process being better in general.
- Etching says no below the thickness rule. The case on record: 55 × 180 µm through-slots in 0.3 mm stock were declined, because 55 µm is about 0.18× the thickness — far below the 0.8–1.2× rule. Thinner stock or a larger feature is the answer, not a harder etch.
Specifications
- Materials for this application: copper and copper alloys. Standard grade H62 brass (UNS C27200); other copper alloy grades sourced to the customer’s specified grade per order. C194/C7025 are not stocked grades here, and beryllium copper is not claimed. Stainless steel, titanium, brass and nickel are etched for other applications; aluminium is not etched.
- Thickness range: 0.05–2.5 mm — gauges 0.05, 0.08, 0.1, 0.12, 0.15, 0.2, 0.25, 0.3, 0.4 and 0.5 mm stocked; above 0.5 mm up to 2.5 mm sourced per order. Lead frames are thin parts: the gauges a lead-frame buyer most often asks for — 0.1, 0.15, 0.2, 0.25 and 0.3 mm — are all stocked.
- Maximum flat sheet: 600 × 1,450 mm — full size only at 0.5 mm and above; thinner gauges run smaller. Lead-frame strips are laid out on flat sheets.
- Tolerance: ±10% of material thickness — on 0.1 mm stock ±0.01 mm; on 0.15 mm stock ±0.015 mm; on 0.2 mm stock ±0.02 mm; on 0.25 mm stock ±0.025 mm; on 0.3 mm stock ±0.03 mm.
- Through-features (lead gaps, slots, singulation openings): ≈ 0.8–1.2× material thickness minimum.
- Half-etch (die-pad steps, grooves, thinned sections): 50–75% of thickness, depth control ±0.05 mm. On 0.2 mm stock, a half-etch step is 0.10–0.15 mm deep.
- Edge quality: burr-free, stress-free, no heat-affected zone — etched edges need no deburring.
- Form: flat sheets only — no coil, no reel. Lead forming (for example gull-wing outer leads) is done through qualified partners and confirmed at quotation.
- Finish: passivation in-house for stainless parts; plating and surface treatment through qualified partners, specified on the drawing.
- Documentation: material test certificate + per-run batch numbers on every order; PPAP Level 3 documentation available; IMDS material data sheets available; NDA signed on request.
- Lead time: samples 3–5 days when material is in stock (7–10 days for special material not stocked); production 7–10 days.
- Commercial: no MOQ; US$100 minimum order; FOB. Monthly capacity is several million parts by count.
What a lead frame is and what it has to do
A lead frame is the metal skeleton inside an IC package. The die sits on the die pad. Fine wires — or, in newer packages, direct attach — connect the die to the inner ends of the leads. The outer ends of the leads are soldered to the printed circuit board. Tie bars hold the whole strip together while it moves through assembly, and are cut away at singulation. Everything the package does electrically and thermally passes through this one thin piece of metal, so its dimensions are not cosmetic: lead width sets resistance, lead spacing sets isolation, and flatness sets whether the package sits down on the board at all.
That is why the manufacturing choice matters before the drawing is released. A lead frame is a precision part, not a bracket: the pattern is dense, the material is thin, and the features are small relative to the thickness. Those three facts are exactly the ones that separate etching from stamping.
How photo-etching makes one
Photo-etching makes a lead frame without touching it. A photoresist pattern is printed on both sides of a flat sheet, and etchant dissolves the exposed metal from both sides at once. There is no die, no punch, no shear — so there is no burr on the edge, no mechanical stress in the thin leads, and no heat-affected zone. The pattern is defined by the film, which means a design change is a new film: the artwork changes, the part changes, and the tooling cost of the change is the cost of a film, not the cost of re-cutting steel.
The same pass that cuts the through-pattern can half-etch selected areas — a die pad stepped down from the lead plane, a groove, a thinned tie-bar section — at 50–75% of the thickness, with depth held to ±0.05 mm. A stamped frame needs a separate coining or milling step for that; an etched frame gets it in the same etch. And because the tooling is digital, prototype and production run on the same tooling: the pilot lot that proves the package is etched the same way as the production lot that follows it.
Where etching wins
Fine pitch. This is the first reason a buyer chooses etching, and it is arithmetic, not preference. A through-feature cannot be etched reliably much below the material thickness — the rule is roughly 0.8–1.2× the thickness. On 0.1 mm stock, a gap between leads floors near 0.08–0.12 mm; on 0.2 mm stock, near 0.16–0.24 mm. So the pitch a buyer can reach is set by the stock they choose, and the stock can be thin: 0.1, 0.15 and 0.2 mm are all stocked gauges. A stamped die holds fine pitch too, but only by cutting a finer die — and a finer die costs more, wears faster, and is less forgiving of a design change. The tolerances post works the ±10% arithmetic for any gauge.
Revisions and prototypes. A lead frame design moves — the die shrinks, a lead count changes, a pad moves. With etching, each revision is a new film and samples are back in 3–5 days. There is no minimum order, so a pilot lot of a few hundred frames can be etched to prove the package before anyone commits to volume. With stamping, each revision is die rework or a new die, and the pilot lot carries the die cost before the design is proven. For a custom IC package that is still being qualified, that difference decides the process.
Complex patterns at no extra cost. In etching, complexity costs nothing extra: a dense, irregular lead pattern etches in the same pass as a simple one, because the etchant does not care how complicated the film is. In stamping, every additional feature is another cut in the die. A lead frame with an irregular die pad, mixed lead widths, or a dense fan-out is an etching part for this reason alone.
Half-etch features. Steps, grooves and recesses at 50–75% depth, controlled to ±0.05 mm, in the same etch as the through-pattern. A die pad stepped down from the lead plane is the standard example. The half-etching post explains the mechanism; the point here is that it is one process step for etching and an extra operation for stamping.
Thin stock, burr-free. Lead frames are thin — most sit in the stocked 0.1–0.3 mm gauges — and thin metal is where stamping struggles most: the punch leaves a burr, the strip carries stress, and the thin leads need deburring. An etched lead comes off the line burr-free and stress-free, which matters twice over: the leads solder cleanly, and the frame stays flat enough to singulate without distortion.
Where stamping wins
Etching does not win everywhere, and a buyer should hear that plainly. Stamping wins when three things are true at once: the design is frozen, the pattern is simple enough for a die to cut cleanly, and the volume is large enough for the die cost to spread thin. A hard die, once cut, stamps fast — and for a standard package running in the millions with no expected revision, it is the economical process. Etching competes on flexibility, not on the unit cost of a frozen high-volume run, and this post does not claim otherwise.
The practical test is the design’s stability. If the drawing is on its third revision this quarter, it is an etching part. If the drawing has not changed in two years and the forecast is a million frames a quarter, get a stamping quote too — and send us the same drawing, so the comparison is against the same pattern.
Where etching says no
The thickness rule is also a refusal rule, and it is better stated here than discovered at quotation. A through-feature floors at roughly 0.8–1.2× the material thickness. The case on record: 55 × 180 µm through-slots in 0.3 mm stock were declined — 55 µm is about 0.18× the thickness, far below the rule, and no etch chemistry makes that reliable. The answer offered was thinner stock or a larger feature, not a promise to try harder.
The same rule applies to lead gaps. A buyer who needs a 0.05 mm gap has two honest options: 0.05 mm stock, where the gap floors near 0.04–0.06 mm, or a wider gap. What a buyer will not get is a guarantee that a gap far below the stock thickness will hold. A drawing that arrives with gaps checked against the rule gets quoted without a round of questions; a drawing that arrives below it gets a DFM note and the same two options. That check costs a day and saves a retest.
Materials and finish
Lead frames are copper and copper-alloy parts. The standard grade here is H62 brass (UNS C27200); other copper alloy grades are sourced to the customer’s specified grade per order — a buyer who specifies a grade gets that grade, quoted as a sourced material rather than a stocked one. C194 and C7025, the two grades packaging buyers ask about most, are not stocked grades here, and this post does not present them as stocked. Beryllium copper is not claimed at all.
Thickness follows the pattern: 0.1, 0.15, 0.2, 0.25 and 0.3 mm are stocked, so a lead frame in those gauges samples in 3–5 days. Heavier gauges up to 2.5 mm are sourced per order. The finish is specified on the drawing: passivation is done in-house for stainless parts, and plating and surface treatment go through qualified partners — the full plating menu is available that way, and the finish is confirmed at quotation rather than assumed. Lead forming, such as gull-wing outer leads, is also a partner step, confirmed at quotation. The etched frame is the lead offer; the finish and the forming are quoted alongside it, not hidden inside it.
What the drawing must carry
A lead-frame drawing that can be quoted without a round of questions carries five things. First, material and thickness: the alloy grade and the gauge — 0.1, 0.2 or 0.3 mm, for example — because thickness sets the tolerance and the minimum gap. Second, the lead pattern with widths and gaps, checked against the 0.8–1.2× thickness rule before it is sent. Third, every half-etch feature with its depth stated as a depth with the ±0.05 mm control, not as a percentage alone. Fourth, a flatness requirement, stated as a number across the strip, because the frame has to sit flat through assembly and singulation. Fifth, the finish and the documentation: the plating or passivation requirement, and the material test certificate and batch-number requirements up front, so they are in the quote rather than added later. The quotations post shows how a drawing moves through the quote; the buyers’ guide shows what to ask before sending one.
FAQ
Should my custom lead frame be etched or stamped?
Etch it when the pitch is fine, the volume is low or uncertain, the design is still moving, or the pattern needs half-etch features. Stamp it when the design is frozen, the pattern is simple, and the volume is large enough for a die to pay for itself. Send the drawing either way — the DFM check will say which process fits it.
What is the finest lead pitch photo-etching can hold?
It follows the thickness rule, not a fixed number. Through-features floor at roughly 0.8–1.2× the material thickness: on 0.1 mm stock a gap floors near 0.08–0.12 mm; on 0.2 mm stock near 0.16–0.24 mm. Lead width carries the ±10% tolerance rule — on 0.2 mm stock, ±0.02 mm. The tolerances post works the arithmetic for any gauge.
Do you etch C194 or C7025 lead frames?
Those grades can be sourced to order, but they are not stocked grades here. The standard stocked grade is H62 brass; a buyer who specifies C194 or C7025 gets it quoted as a sourced material, with the lead time that sourcing carries.
Can you half-etch the die pad or add grooves?
Yes — half-etching is part of the etching process. Steps, grooves and recesses run at 50–75% of thickness with depth controlled to ±0.05 mm, in the same etch as the through-pattern. A die pad stepped down from the lead plane is the standard example.
How fast can I get prototype lead frames?
Samples in 3–5 days when the gauge is in stock, production in 7–10 days, no minimum order. A design revision is a new film, so a revised prototype follows in the same 3–5 day loop.
Do etched lead frames need deburring?
No. Etched edges are burr-free and stress-free, with no heat-affected zone — the leads come off the line ready to solder, and the frame stays flat for singulation.
Do you etch aluminium lead frames?
No. Aluminium is the one metal we do not etch. Lead frames are copper and copper-alloy parts, etched from flat sheets — no coil, no reel.
- What Does a 770 W/cm² GPU Hotspot Mean for the Etched Copper Flow Layer? - November 22, 2026
- Photo-Etched Precision Medical Metal Components: Micro-Needles, Lancets and Microfluidic Parts - November 21, 2026