On November 11, 2026, Frore Systems was named a CES Innovation Awards 2027 honoree for LiquidJet, its direct-to-chip liquid coldplate for AI data centres — the company’s fourth consecutive CES Innovation Award, in a program that drew nearly 4,000 submissions. The headline number in the announcement is a hotspot power density of 770 W/cm², managed by LiquidJet Diamond, the version with an integrated diamond spreader. Frore says the standard LiquidJet manages 670 W/cm², lets a GPU run up to 12°C cooler and delivers up to 25% more AI tokens per watt; the Diamond version goes to up to 22°C cooler and up to 35% more tokens per watt.
That number is a demand signal, not a product claim for this post. Frore builds LiquidJet with what it describes as a semiconductor manufacturing process adapted to metal wafers — not photo-chemical etching — and Frore is not a customer of ours. What the number does tell a buyer is where the heat is going: GPU dies are getting larger and their power is concentrating into smaller hotspots, and the thin metal layer that carries coolant across the die has to keep up. This post answers the question that follows from that: what does a 770 W/cm² hotspot demand of the etched copper flow layer — the channel size, the material, the thickness and the tolerance a drawing has to carry?
The short answer is that the flow layer gets thinner, finer and more copper, not thicker and coarser. Hotspot density pushes channel features toward the etching floor, pushes the layer toward thin copper stock, and pushes the tolerance budget toward the ±10% rule worked on thin gauges. The rest of this post puts numbers on each of those pushes, so a buyer can check a drawing against them before it is released.
ANSWER CAPSULE — six things a buyer needs
- 770 W/cm² is Frore’s number, and it is a trend marker. Frore says LiquidJet Diamond manages hotspots up to 770 W/cm² (670 W/cm² for the standard LiquidJet), demonstrated at the OCP Global Summit cooling the 2300W NVIDIA Rubin. The direction is clear: die power is concentrating into smaller, hotter spots, and the flow layer above the die has to remove heat from a smaller area.
- The flow layer is an etched copper layer. A flow plate is a thin copper sheet with a patterned channel field: through-etched passages that become enclosed channels when layers are joined, and half-etched channels where the depth is specified. Copper is the material because it is the only one validated here for coolant (PG water and deionised water) — stainless steel, nickel and titanium are not named for coolant service.
- The channel floor is the thickness rule. A through-feature floors at roughly the material thickness (0.8–1.2× as a rule of thumb). On 0.2 mm copper a through-feature floors near 0.16–0.24 mm; on 0.3 mm, near 0.24–0.36 mm. A finer channel needs thinner stock, not a harder etch.
- Half-etching sets the channel depth. Shallow channels are half-etched to 50–75% of thickness with depth held to ±0.05 mm. On 0.3 mm stock a half-etch channel is 0.15–0.225 mm deep — a number the buyer specifies and the etcher holds, not a second operation with its own tolerance stack.
- Tolerance is ±10% of thickness, worked on thin gauges. On 0.2 mm stock that is ±0.02 mm; on 0.3 mm stock, ±0.03 mm; on 0.5 mm stock, ±0.05 mm. A buyer who needs a tighter callout on a thick gauge is asking for more than the process holds on that gauge — the answer is thinner stock or a separate conversation, never a promised figure the process cannot hold.
- Etching says no below the thickness rule. The case on record: 55 × 180 µm through-slots in 0.3 mm stock were declined, because 55 µm is about 0.18× the thickness — far below the 0.8–1.2× rule. Thinner stock or a larger feature is the answer, not a harder etch.
Specifications
- Materials for this application: copper for coolant-wetted flow layers (validated for coolant media: PG water / deionised water). Stainless steel, titanium, brass and nickel are etched for other applications, but are not specified here for coolant service. Aluminium is not etched.
- Thickness range: 0.05–2.5 mm — gauges 0.05, 0.08, 0.1, 0.12, 0.15, 0.2, 0.25, 0.3, 0.4 and 0.5 mm stocked; above 0.5 mm up to 2.5 mm sourced per order. Flow layers are thin parts: the gauges a buyer most often asks for — 0.1, 0.15, 0.2, 0.25 and 0.3 mm — are all stocked.
- Maximum flat sheet: 600 × 1,450 mm — full size only at 0.5 mm and above; thinner gauges run smaller. Flat sheet only — no coil, no reel.
- Tolerance: ±10% of material thickness — on 0.1 mm stock ±0.01 mm; on 0.2 mm stock ±0.02 mm; on 0.3 mm stock ±0.03 mm; on 0.5 mm stock ±0.05 mm.
- Through-features (channels, slots, apertures, inlet/outlet ports): ≈ 0.8–1.2× material thickness minimum.
- Half-etch (flow channels, grooves, stepped relief): 50–75% of thickness, depth control ±0.05 mm. On 0.3 mm stock, a half-etch channel is 0.15–0.225 mm deep.
- Edge quality: burr-free, stress-free, no heat-affected zone — etched channel walls need no deburring, which matters when the wall is the flow boundary.
- Finish: passivation in-house for stainless parts; plating and surface treatment through qualified partners, specified on the drawing. No fuel-cell coatings.
- Documentation: material test certificate + per-run batch numbers on every order; PPAP Level 3 documentation available; IMDS material data sheets available; NDA signed on request.
- Lead time: samples 3–5 days when material is in stock (7–10 days for special material not stocked); production 7–10 days.
- Commercial: no MOQ; US$100 minimum order; FOB.
What Frore announced, and what it is not
The announcement itself is straightforward. Frore Systems, a Silicon Valley company with manufacturing operations in Taiwan, won its fourth consecutive CES Innovation Award for LiquidJet, a direct-to-chip 3D ultra short-loop, multi-stage coldplate. Frore describes the design as a 3D ultra short-loop multi-stage channel layout that can be customised to the power map of each GPU, including extreme hotspots, and says it is fabricated by adapting semiconductor manufacturing processes to metal wafers. That last point matters for this post: LiquidJet is not a photo-etched part, and this post does not claim otherwise. The coldplate Frore sells and the etched copper flow layer a buyer sources from an etching house are different layers of the same thermal problem, made by different processes.
The numbers Frore puts on the problem are worth reading as a trend, because they are the numbers a flow-layer drawing has to survive. LiquidJet, Frore says, lets GPUs run up to 12°C cooler and delivers up to 25% more AI tokens per watt, managing hotspot power density of 670 W/cm². LiquidJet Diamond adds an integrated diamond spreader embedded in the coldplate base, positioned at the hotspot locations, and Frore says it delivers up to 22°C cooler, up to 35% more tokens per watt, and hotspots up to 770 W/cm². At the OCP Global Summit in October 2026, Frore demonstrated the plates cooling the 2300W NVIDIA Rubin at that 770 W/cm² hotspot density. Frore’s own release also notes the die-size spread behind the trend: from the 1,488 mm² NVIDIA Blackwell Ultra to the 46,225 mm² Cerebras Wafer-Scale Engine, roughly thirty times the footprint. And in its white paper Cooling Is the Next Revolution, Frore’s research argues that optimising the full thermal stack could produce over 40% more AI tokens from the same electricity — Frore’s research, attributed here, not a factory figure.
The takeaway for a buyer is not the award. It is that the heat a flow layer has to remove is concentrating: bigger dies, higher total watts, and the worst of it packed into a smaller hotspot. The layer above the die has to carry more heat through a thinner, finer-patterned sheet. That is a specification problem, and it is the problem the rest of this post works through.
What 770 W/cm² does to the flow layer
A coldplate is a stack, and the etched copper flow layer is one layer of it: the patterned sheet that defines where coolant goes. When the hotspot density rises, three things happen to that layer, and all three push in the same direction — thinner, finer, more precise.
First, the channel field gets denser. A hotspot is a small area dumping a large share of the die’s power, so the coolant has to reach that area and leave it quickly. That means more channels, closer together, with narrower walls between them. Etching’s advantage here is repeatability: the same film makes every channel the same way, with no tool wear changing the ten-thousandth channel relative to the first — the pilot-lot repeatability measurements show the pattern holding across a production lot. The wall between two channels is a ligament of etched copper, and its minimum width is governed by the same thickness rule as any other feature: a ligament much narrower than the material is thick is not a reliable etched feature. On 0.3 mm stock, a wall much below about 0.24–0.36 mm is asking the process for something it does not reliably do. The answer is thinner stock — on 0.2 mm stock the floor drops to about 0.16–0.24 mm — not a request to etch finer than the rule allows.
Second, the layer gets thinner. A thin flow layer puts the coolant closer to the die and keeps the stack short, which is why flow layers sit in the stocked thin gauges — 0.1, 0.15, 0.2, 0.25 and 0.3 mm — rather than at the thick end of the range. But thinner stock also means the tolerance arithmetic gets tighter in absolute terms: ±10% of 0.2 mm is ±0.02 mm, and the drawing has to be written for that number, not for a tolerance the process holds on a thicker gauge. A buyer who writes ±0.05 mm on a 0.2 mm flow layer is asking for two and a half times the precision the process holds on that gauge; the conversation that follows should be about thinner stock, a different route for the tightest features, or a conditional conclusion — never a promised figure.
Third, the channel depth becomes a specified number rather than a by-product. A flow channel is usually a half-etch: a shallow recess cut to 50–75% of the thickness, with depth controlled to ±0.05 mm. On 0.3 mm stock that is a channel 0.15–0.225 mm deep. The depth is the number that sets the flow cross-section, so it belongs on the drawing as a dimension with its own tolerance, not as a note that says “half-etch”. The half-etching guide works through the same depth rule for channels, fold lines and stepped features; the flow-layer version of it is the same arithmetic applied to a coolant path.
None of this is a claim about what an etched layer can cool. No heat-flux, pressure-drop or thermal-resistance figure for an etched part appears in this post, because none has been measured for one. The point is narrower and checkable: as hotspot density rises, the drawing’s numbers — feature size, thickness, depth, tolerance — all have to be written against the etching rules, and a drawing that violates them will come back with questions instead of a price.
Why the flow layer is copper, and only copper
Coolant-wetted plates are specified in copper here for one reason: copper is the only material this factory has validated for coolant media — PG water and deionised water — and for electrolytic media. Stainless steel, nickel and titanium are etched for other applications, and they are good materials, but they have not been validated for coolant service, so they are not named for it in this post. A buyer who asks for a stainless flow plate for a water loop is asking for a material decision the factory has not validated, and the quotation should say so rather than substitute a material on the strength of a datasheet.
Copper also brings the practical advantage that matters in a flow layer: it etches cleanly into fine, repeated patterns with burr-free edges, so the channel walls need no deburring — and a deburred channel wall is a different wall, with a different flow cross-section, than the one on the drawing. The copper and brass guide sets out what changes when the material changes from stainless steel to copper; the flow-layer version of that choice is made on coolant validation first and etch behaviour second.
One more material boundary, stated plainly: aluminium is not etched. A flow layer that has to be aluminium is not an etched part from this factory, and the right answer is to say so before the drawing is released.
The numbers that decide the drawing
Four numbers decide whether a flow-layer drawing can be quoted as drawn, and all four are arithmetic from the factory rules.
Thickness. The layer’s stock gauge sets everything else. The stocked gauges run 0.05–0.5 mm; above 0.5 mm up to 2.5 mm is sourced per order. A flow layer at 0.2 or 0.3 mm is a stocked gauge, which is why samples can be quoted in 3–5 days. The full 600 × 1,450 mm sheet size applies only at 0.5 mm and above; thinner gauges run smaller, so a large-area flow layer on thin stock is quoted in the format the gauge allows, not the maximum.
Minimum feature. The thickness rule: a through-feature floors at roughly 0.8–1.2× the material thickness. On 0.2 mm stock, a through-slot or port floors near 0.16–0.24 mm; on 0.3 mm, near 0.24–0.36 mm; on 0.5 mm, near 0.4–0.6 mm. The recorded case is the 55 × 180 µm through-slots in 0.3 mm stock that were declined — 55 µm is about 0.18× the thickness, far below the rule. A flow field whose narrowest channel or ligament sits below the floor needs thinner stock or a larger feature, and the drawing should be revised before quotation rather than after.
Tolerance. The standard is ±10% of material thickness: ±0.01 mm on 0.1 mm stock, ±0.02 mm on 0.2 mm, ±0.03 mm on 0.3 mm, ±0.05 mm on 0.5 mm. The channel width, the ligament width and the port diameter are all judged against that rule. A tighter callout on a dimension that matters — a metering orifice, a sealing land — needs a separate conversation before it goes on the drawing.
Channel depth. Half-etch channels run 50–75% of thickness with depth control of ±0.05 mm. On 0.3 mm stock that is 0.15–0.225 mm deep; on 0.2 mm stock, 0.10–0.15 mm deep. Deeper than 75% risks breakthrough, so a channel that needs to be deeper than the rule allows is a different design — a through-etched passage with a cover layer, or a thicker stock with a revised depth — not a request to push the half-etch deeper.
The four things a flow-layer drawing must carry
A quotation that covers the part needs four things on the drawing, and a drawing that lacks one of them will come back with questions instead of a price. The buyer’s guide and the quotations guide cover the same four points for etched parts generally; the flow-layer version is as follows.
First, material and grade, to the customer’s specification — copper for a coolant-wetted layer, with the grade named. The etcher stocks the gauges, not the customer’s grade. Second, thickness, with the gauge named rather than implied, because the gauge sets the feature floor, the tolerance and the channel depth. Third, the minimum feature size stated next to the thickness — the narrowest channel, the thinnest ligament, the smallest port — so the thickness rule can be checked on the face of the drawing. Fourth, the tolerance callouts that matter, the channel depth with its ±0.05 mm control, the finish, and the inspection requirement. A drawing that carries those four things gets a quotation; a drawing that does not gets a round of questions first.
The same discipline applies to the chip itself. The lead-frame post covers precision etching for IC packaging — fine, flat, repeatable parts where the drawing carries the same four things. A flow layer is the thermal counterpart of that logic: the same process, the same rules, applied to the sheet that carries coolant instead of the frame that carries the die.
Where etching stops
Three limits, stated plainly. First, the thickness rule: a through-feature cannot be etched reliably much below the material thickness, and a ligament much narrower than the thickness is not a reliable feature either. The fix is thinner stock or a larger feature, never a harder etch. Second, the tolerance rule: ±10% of thickness, so a buyer who needs ±0.05 mm on a 1.0 mm part is asking for twice the precision the process holds on that gauge. Third, the form limit: flat sheet only, 600 × 1,450 mm maximum, no coil and no reel. A flow layer that needs a formed, deep-drawn or tubular form is not an etched flat part.
There is a fourth limit that matters for a cold plate specifically. An etched flow layer is a layer, not a sealed cold plate. A finished welded cold-plate assembly — diffusion-bonded or brazed, sealed and pressure-tested — can be arranged through qualified partners for larger orders, but it is not made in-house and it is not the standard etched-plate quote. A buyer who needs the finished assembly should say so at quotation, so the quote covers the assembly route rather than the layer alone. And a buyer who needs the etched layer only — the patterned copper sheet, ready to be joined into their own stack — gets exactly that: the layer, etched, with a material test certificate and a per-run batch number, in 3–5 days for samples and 7–10 days for production.
FAQ
- Is LiquidJet made by photo-etching? No. Frore states LiquidJet is built with a semiconductor manufacturing process adapted to metal wafers. This post uses Frore’s announcement as the demand signal — hotspot density is rising — and describes the etched copper flow layer as the answering capability for buyers who source that layer by etching. Frore is not a customer of ours, and nothing here claims Xinketching makes LiquidJet.
- What does 770 W/cm² mean for my flow-layer drawing? It means the channel field gets denser and the walls get thinner, which pushes the drawing toward the etching floor: the narrowest channel and the thinnest ligament must respect the thickness rule (about 0.8–1.2× the material thickness), and the channel depth must be specified as a half-etch (50–75% of thickness, ±0.05 mm). A drawing that violates the floor will come back with questions.
- What is the smallest channel etching can make in a copper flow layer? About the material thickness: on 0.2 mm stock, through-features floor near 0.16–0.24 mm; on 0.3 mm stock, near 0.24–0.36 mm. Finer channels need thinner stock, not a harder etch.
- Why copper, and not stainless steel, for a coolant plate? Because copper is the only material validated here for coolant media (PG water and deionised water) and electrolytic media. Stainless steel, nickel and titanium are etched for other applications but have not been validated for coolant service, so they are not specified for it here.
- Can etching make the shallow flow channels, or only through-holes? Both, in the same etch: through-passages cut from both sides, and shallow channels half-etched to 50–75% of thickness with depth held to ±0.05 mm. On 0.3 mm stock a half-etch channel is 0.15–0.225 mm deep.
- What tolerance can I design to? ±10% of material thickness: ±0.02 mm on 0.2 mm stock, ±0.03 mm on 0.3 mm stock, ±0.05 mm on 0.5 mm stock. A tighter callout needs a separate conversation before it goes on the drawing.
- Can you supply the finished sealed cold plate, not just the etched layer? A finished welded (diffusion-bonded or brazed) sealed cold plate can be arranged through qualified partners for larger orders. It is not made in-house and is quoted as a separate assembly route — say so at quotation if that is what you need.
- How fast are samples and production? Samples in 3–5 days when the material is in stock (7–10 days for special material not stocked); production 7–10 days. No MOQ; US$100 minimum order; FOB.
The bottom line for a cold-plate buyer
A 770 W/cm² hotspot does not change what photo-etching is. It changes what the drawing has to carry: a denser channel field, thinner copper, a specified half-etch depth, and a tolerance budget worked on thin gauges. If the layer is a thin copper sheet with a patterned channel field, etching is the process that makes it — burr-free, stress-free, repeatable, with the same digital tooling from prototype to production. If the narrowest feature sits below the thickness rule, or the material has to be aluminium, or the part has to be a formed tube, it is not an etched part, and the right answer is to say so before the drawing is released. Send the drawing with the material and grade, the thickness, the smallest feature and the channel depth, and the quotation will answer the question the drawing actually asks. For a flow-layer quotation, contact sales@xinketching.com.
- How to Specify a Photo-Etched Encoder Disc: Tolerance, Material, and Slot Width on the Drawing - November 23, 2026
- Top 8 Metal Etching Factories In Japan (In-Depth Analysis 2025) - November 23, 2026
- What Does a 770 W/cm² GPU Hotspot Mean for the Etched Copper Flow Layer? - November 22, 2026