An encoder disc looks simple on a drawing: a thin metal circle with slots around it. The buying decision is not simple, because every number on that drawing interacts with the others. Slot width, web width, material thickness, tolerance, bore size and flatness are one system, and a drawing that over-specifies one of them while leaving another open is how a disc arrives on time and still reads badly.
This post answers the question a buyer asks before the drawing is released: what numbers do I put on the drawing for a photo-etched encoder disc, and which numbers will the supplier push back on? Every figure below comes from one factory’s working rules — Xinketching, Dongguan, photo etching since 2005 — so you can check a drawing against it line by line.
Answer capsule
- The drawing carries four things: material and temper, thickness, tolerance band, and quantity — plus the datum that locates the track to the shaft. If any of the four is missing, the quote comes back with a question instead of a price.
- Tolerance is ±10% of material thickness. On 0.1 mm stock that is ±0.01 mm; on 0.2 mm stock ±0.02 mm; on 0.5 mm stock ±0.05 mm. There is no flat ±0.01 mm claim across all thicknesses.
- Slot width and web width floor at roughly 0.8–1.2× the material thickness. On 0.2 mm stock, neither a slot nor the web between two slots should go below about 0.16–0.24 mm.
- Slot count follows the track circumference. At a Ø100 mm track diameter and 0.40 mm pitch, about 785 slots fit. The worked table is below.
- Materials: stainless steel and nickel are the usual choices; titanium where weight and corrosion matter; copper alloys where electrical behaviour matters. Aluminium is not etched.
- Limits: maximum disc diameter Ø600 mm; flat sheet up to 600 × 1,450 mm (full size only at 0.5 mm and above). Samples in 3–5 days, production in 7–10 days, no minimum order, minimum order charge US$100.
Specifications
| Item | Specification |
|---|---|
| Materials | Stainless steel, nickel, titanium, copper alloys, brass. Aluminium is not etched. |
| Thickness range | 0.05–2.5 mm. Stocked gauges: 0.05, 0.08, 0.1, 0.12, 0.15, 0.2, 0.25, 0.3, 0.4, 0.5 mm. Above 0.5 mm up to 2.5 mm sourced per order. |
| Etch tolerance | ±10% of material thickness (0.1 mm → ±0.01 mm; 0.15 mm → ±0.015 mm; 0.2 mm → ±0.02 mm; 0.3 mm → ±0.03 mm; 0.5 mm → ±0.05 mm). Raw-stock thickness tolerance is a separate ±0.02 mm — do not conflate the two. |
| Through-feature floor | Slot width and web width each ≥ ~0.8–1.2× material thickness. |
| Maximum disc diameter | Ø600 mm. |
| Maximum flat sheet | 600 × 1,450 mm, full size only at 0.5 mm and above; thinner gauges run in smaller formats. |
| Half-etch | Depth 50–75% of thickness, depth control ±0.05 mm (on 0.2 mm stock, a half-etched step is 0.10–0.15 mm deep). |
| Edge quality | Burr-free, stress-free, no heat-affected zone. No deburring step. |
| Flatness | Specified against the read-head gap and the mounting method, not as a standalone number — state the gap on the drawing. |
| Lead times | Samples 3–5 days; production 7–10 days. |
| Order terms | No minimum order quantity; minimum order charge US$100. FOB. |
| Documentation | Material test certificate (MTC) and per-run batch/lot traceability on every order. PPAP Level 3 available. IMDS data sheets on request. NDA signed on request. |
What the drawing must carry
A usable encoder-disc drawing carries four things, and a fifth that is often left open. Material and temper — name the alloy, and the temper if the disc will be formed or handled after etching. Thickness — a single nominal value from the stocked gauge list where possible; an off-list gauge is sourced per order and costs a question, not a refusal. Tolerance band — write it as ±10% of the stated thickness, with the worked figure next to it (for example, “±0.02 mm on 0.2 mm stock”), so the shop floor and the inspector read the same number. Quantity — prototype lot and annual volume, because the same disc is etched for a prototype and stamped only when the design freezes and the volume justifies a die. The datum — which feature locates the track to the shaft: usually the centre bore or the bolt-circle pattern. An outer diameter should be the datum only if it actually performs the locating function in the assembly; in most robot-joint and instrument builds it is only a handling edge.
If the bore is the datum, the drawing should control the bore, the track, and the relationship between them as one system: bore size and roundness, radial position of the track to the bore, mounting-hole position, allowable bore clearance, and the assembly method used to centre the disc. A chain of coordinate dimensions from an arbitrary edge hides that relationship. Basic dimensions from a common datum system, with a position or runout requirement that matches the assembly, are clearer — and they give the supplier something it can actually inspect.
Tolerance, worked out
The ±10% rule is the whole tolerance story for etched features, and it is worth writing out because buyers often carry a flat tolerance from a machined part onto an etched one. On 0.1 mm stock the band is ±0.01 mm. On 0.15 mm stock it is ±0.015 mm. On 0.2 mm stock it is ±0.02 mm. On 0.3 mm stock it is ±0.03 mm. On 0.5 mm stock it is ±0.05 mm. The band grows with the material because the chemistry removes a proportion of the thickness, not a fixed amount.
Two things buyers get wrong. First, the raw material itself carries its own thickness tolerance of ±0.02 mm, which is separate from the etch tolerance — a 0.2 mm sheet can arrive at 0.18–0.22 mm before etching starts, and the etch band applies on top of the actual stock. Second, tightening only the etched-pattern tolerance does not remove the clearance between the disc and its hub. Total runout at the scale track combines pattern placement, bore position, bore clearance, hub fit, fastener shift and disc flatness. If the disc is located by a loose bore, no pattern tolerance will fix the reading.
Slot width, web width, and how many slots fit
Photochemical etching opens an aperture from both faces, and the sidewall is not perfectly vertical: lateral etching creates undercut, so a narrow slot in thick material comes out with a visible difference between the mask opening and the finished entrance and exit. That is why slot width, web width and material thickness must be reviewed together, and why the floor for both is roughly the material thickness — 0.8–1.2× as a working rule.
The table below is arithmetic, not a catalogue claim. Pitch is slot width plus web width, and the slot count is the track circumference divided by the pitch.
| Stock thickness | Slot floor (≈0.8–1.2×) | Web floor (≈0.8–1.2×) | Pitch floor (≈2× thickness) | Slots on a Ø100 mm track at that pitch |
|---|---|---|---|---|
| 0.1 mm | 0.08–0.12 mm | 0.08–0.12 mm | 0.16–0.24 mm | ~1,310–1,960 (at 0.20 mm pitch: ~1,570) |
| 0.15 mm | 0.12–0.18 mm | 0.12–0.18 mm | 0.24–0.36 mm | ~870–1,310 (at 0.30 mm pitch: ~1,047) |
| 0.2 mm | 0.16–0.24 mm | 0.16–0.24 mm | 0.32–0.48 mm | ~650–980 (at 0.40 mm pitch: ~785) |
| 0.3 mm | 0.24–0.36 mm | 0.24–0.36 mm | 0.48–0.72 mm | ~435–650 (at 0.60 mm pitch: ~524) |
| 0.5 mm | 0.40–0.60 mm | 0.40–0.60 mm | 0.80–1.20 mm | ~260–390 (at 1.00 mm pitch: ~314) |
Two consequences follow. First, a thinner disc buys a finer pattern: dropping from 0.2 mm to 0.1 mm stock roughly doubles the slot count at the same track diameter. Second, the trade is handling: a very thin disc can dish during handling or coating, while a thicker disc is rigid but pushes narrow slots against the process floor. The choice is a stiffness decision as much as a resolution decision, and it should consider disc diameter, unsupported span, hub design, temperature and optical finish together.
The same arithmetic scales up. On the largest disc this factory etches, Ø600 mm, a track at Ø550 mm has a circumference of about 1,728 mm. At 0.2 mm stock and 0.40 mm pitch that is about 4,320 slots. If the design needs more transitions than the pitch floor allows at that diameter, the answer is thinner stock or a larger track diameter — not a tighter etch.
State on the drawing where the critical slot width is measured. For a transmissive reader, the entrance dimension, the exit dimension and the projected optical opening are not the same number once undercut is in play. Naming the measurement face on the drawing removes the most common inspection argument before it starts.
Transmissive or reflective — the choice that changes the drawing
Before material or thickness, the drawing should say how the sensor reads the disc, because that decides whether the slots go all the way through. A transmissive head reads light through open slots, so the track is a through-etched pattern and the slot/web floor above applies in full. A reflective head reads contrast off the surface, so the track can be a half-etched pattern — a recessed zone 50–75% of the thickness deep, with depth controlled to ±0.05 mm — and the through-feature floor does not apply to the pattern itself. An incremental track counts transitions from a reference mark; an absolute track carries a coded pattern that reports position directly. The read-head type, the track type and the slot geometry belong on the drawing together, because each constrains the other two.
Material: four options and when each wins
Stainless steel is the default for most encoder discs: it combines corrosion resistance, stiffness and dimensional stability in thin sections, and it patterns cleanly. Nickel is chosen for specialised environments where its properties are needed rather than as a general substitute. Titanium earns its place where weight and corrosion resistance dominate — aerospace and instrumentation discs — and it etches in the same 0.05–2.5 mm range. Copper alloys are useful where electrical behaviour matters rather than for the optical track itself. The choice should weigh operating temperature, humidity, assembly method and the stiffness needed to prevent flutter at speed, not only the pattern. Aluminium is the one material this factory does not etch, so an aluminium disc is a different supplier’s job.
Mounting: bore, bolt circle, or adhesive
The mounting decision is part of the accuracy budget. A centre bore used as the datum needs its size, roundness and position to the track controlled as a system, and the drawing should state the allowable bore clearance and the hub fit — clearance here is a position error, not a tolerance footnote. A bolt-circle pattern can locate the disc when the bore is only a clearance hole; then the hole positions, not the bore, control the track. Adhesive mounting avoids fastener shift but moves the accuracy question to the bonding fixture and the cure cycle. Temporary handling tabs or an outer carrier can protect a delicate disc through etching and cleaning and separate at assembly; if the design needs them, they should be on the drawing as temporary features, not discovered on the shop floor.
Inspection: agree it before the first article
Do not specify concentricity without a measurement method. A vision system can fit a circle through selected slot centres relative to the datum bore. A functional gauge can reproduce the hub fit. A coordinate machine is useful for mounting features but inefficient for thousands of narrow apertures. Agree on which slots are sampled, how the fitted circle is calculated, and whether the disc is measured free, vacuum-held or clamped — a thin disc reads differently under each condition. Pilot-lot measurement exists for exactly this reason: a first lot is measured for repeatability before the production quantity is committed. Every production run ships with a material test certificate and batch traceability, and PPAP Level 3 documentation is available where the customer’s process requires it.
Where etching says no
Four lines this factory will not cross, stated plainly so a buyer does not spend a design cycle on them. A slot or web below the thickness floor. The case on record: 55 × 180 µm through-slots in 0.3 mm stainless steel were declined, because 55 µm is about 0.18× the thickness — far below the 0.8–1.2× rule. Thinner stock or a larger feature is the answer. A disc above Ø600 mm. The maximum etched disc diameter is Ø600 mm; a larger code wheel needs a different construction. Aluminium. Not etched here, in any thickness. A pattern that needs a tolerance the chemistry cannot hold. The ±10% rule is the band; a drawing that demands ±0.01 mm on 0.5 mm stock (a ±0.05 mm band) is asking for a process this factory does not run.
What to send for a quote
Send the drawing with the four elements — material and temper, thickness, tolerance band, quantity — plus the track diameter, the slot and web widths, the read-head type (transmissive or reflective), the datum feature, and the flatness zone with the sensor gap. A DXF or STEP of the pattern is enough to check the pitch against the thickness rule the same day. Samples run 3–5 days; production 7–10 days; there is no minimum order quantity and the minimum order charge is US$100. If the numbers above show the design is outside the etching window, the honest answer is thinner stock, a larger feature, or a different process — and it is better to get that answer before the drawing is released than after the first article.
FAQ
What is the finest slot an etched encoder disc can hold? About 0.8–1.2× the material thickness for both the slot and the web between slots. On 0.1 mm stock that is roughly 0.08–0.12 mm; on 0.2 mm stock, roughly 0.16–0.24 mm. Anything finer needs thinner stock or a different process.
What tolerance should I put on the drawing? ±10% of material thickness: ±0.01 mm on 0.1 mm stock, ±0.02 mm on 0.2 mm stock, ±0.05 mm on 0.5 mm stock. The raw stock itself carries a separate ±0.02 mm thickness tolerance.
What is the largest encoder disc you etch? Ø600 mm maximum disc diameter. A track at Ø550 mm on that disc holds about 4,320 slots at 0.40 mm pitch on 0.2 mm stock.
Which material should I choose? Stainless steel for most discs; nickel for specialised environments; titanium where weight and corrosion matter; copper alloys where electrical behaviour matters. Aluminium is not etched.
Transmissive or reflective — does it change the price? It changes the drawing, not the process family. Transmissive discs need through-slots at the pitch floor; reflective discs can use a half-etched pattern 50–75% of the thickness deep, with depth controlled to ±0.05 mm.
How fast can I get prototype discs? Samples in 3–5 days, production in 7–10 days. There is no minimum order quantity and the minimum order charge is US$100.
Do etched encoder discs need deburring? No. Etched edges are burr-free, stress-free and have no heat-affected zone, so there is no deburring step before assembly.
Xinketching — precision photo-etched parts, Dongguan, since 2005. Send a drawing to sales@xinketching.com and the pitch will be checked against the thickness rule before a price is quoted.
Further reading
- Encoder discs and code wheels
- Etching vs stamping vs laser
- How photo etching works
- Metal etching services
- Drawing revision: how a drawing is checked before release
- How to Specify a Photo-Etched Encoder Disc: Tolerance, Material, and Slot Width on the Drawing - November 23, 2026
- Top 8 Metal Etching Factories In Japan (In-Depth Analysis 2025) - November 23, 2026
- What Does a 770 W/cm² GPU Hotspot Mean for the Etched Copper Flow Layer? - November 22, 2026