Every gram on an aircraft is a line item. A shim that sets a gap, a bracket that holds a line or a sensor in place — each one is small, but there are hundreds of them, and their weight adds up the same way their tolerances do. Titanium earns its place in aircraft for two plain reasons: it is strong for its weight, and it does not corrode the way steel does in the environments an airframe lives in. The question for a buyer is not whether titanium is a good aircraft metal. It is whether etching is the right way to make a thin titanium shim or bracket — and what to put on the drawing so the part comes back right the first time.
A July 2026 industry guide to titanium etching machines puts the process problem first: titanium’s thin titanium-dioxide layer forms within milliseconds of exposure to air, and it shrugs off most conventional etchants. The chemistries that do work are hydrofluoric-acid blends, typically HF with nitric acid, run at room temperature — the guide quotes roughly 15–25 µm/min in a typical HF/HNO3 blend. That is the equipment maker’s figure, not ours, and it explains why titanium etching is a controlled-chemistry job rather than a standard etch run. It also lists aerospace brackets among the applications where titanium etching has no real alternative. Fotofab’s aerospace page makes the same point from the buyer’s side: photo-etched parts for avionics housings, sensors, connectors and shielding, plus shims for tolerance absorption — thin, precise, repeatable parts where a machined or stamped alternative is either too heavy, too stressed, or too expensive to revise.
Answer capsule: six things a buyer needs
- We etch titanium. Titanium is one of the five metals we photo-etch — stainless steel, titanium, copper, brass and nickel. We do not etch aluminium.
- A shim is etching’s home ground; a bracket is a flat profile. Shims are flat, thin, and tolerance-critical — exactly what photo etching does best. A bracket is etched as a flat profile with its holes, slots and outline cut in one pass; if the design needs a bend, that forming step is outsourced and must be confirmed at quotation.
- Weight is a material property you specify, not a claim we make. Titanium’s density is ≈ 4.5 g/cm³, against ≈ 7.9 g/cm³ for steel. On the same outline and thickness, a titanium shim weighs little more than half its steel equivalent. The saving is arithmetic, not marketing.
- Tolerance is ±10% of thickness. On 0.1 mm stock that is ±0.01 mm; on 0.2 mm stock, ±0.02 mm; on 0.5 mm stock, ±0.05 mm. A shim’s whole job is its thickness — so its tolerance is the number the assembly is built around.
- The feature floor is the thickness rule. A through-feature floors at roughly the material thickness (0.8–1.2×). A 0.20 mm hole in 0.3 mm stock is a case we declined — the same rule governs a bracket’s mounting holes and lightening slots: finer features need thinner stock, not a harder etch.
- Etching leaves no stress and no burr. No cutting force, no heat-affected zone, no burr on the edge. A thin titanium part comes off the line flat — and a design revision is new artwork, not new tooling.
Specifications
- Materials: stainless steel, titanium, copper, brass, nickel (we do not etch aluminium)
- Titanium grades etched: commercially pure Grades 1 and 2 and alloy Grade 5 (Ti-6Al-4V); Grade 2 is the usual choice for corrosion-exposed shims, Grade 5 the higher-strength choice for brackets
- Thickness range: 0.05–2.5 mm — gauges 0.05, 0.08, 0.1, 0.12, 0.15, 0.2, 0.25, 0.3, 0.4 and 0.5 mm stocked; above 0.5 mm up to 2.5 mm sourced per order. Shim stock 0.1–2.5 mm held in stock
- Maximum flat sheet: 600 × 1,450 mm — full size only at 0.5 mm and above; thinner gauges run smaller
- Tolerance: ±10% of material thickness
- Half-etch (weight pockets, recesses): 50–75% of thickness, depth control ±0.05 mm
- Through-features: ≈ 0.8–1.2× material thickness minimum (0.20 mm hole in 0.3 mm stock declined)
- Form: flat sheets only — no coil, no reel; bending/forming outsourced, confirm at quotation
- Finish: passivation available in-house; plating and surface treatment outsourced
- Lead time: samples 3–5 days when material is in stock (7–10 days for special material not stocked); production 7–10 days
- Commercial: no MOQ; US$100 minimum order; FOB; material test certificate + per-run batch numbers on every order; PPAP Level 3 documentation available
Why a shim is the etched part, and a bracket is the flat profile
A shim does one job: it fills a gap to a known thickness. Its value is entirely in that thickness and in staying flat — a shim that is dished, burred or stressed will not sit true, and the assembly it spaces will not sit true either. Photo etching cuts the outline, the holes and the slots chemically, with no tool pressing on the sheet and no heat going into it, so a 0.1 mm titanium shim comes out flat and stress-free, with a clean edge that will not shed a burr into the joint. The same artwork produces the first article and the ten-thousandth, so a shim set ordered in January matches the set ordered in June. Our tolerances post works through the ±10% arithmetic; our titanium guide covers grade choice in general.
A bracket is a different shape with the same discipline. The etched bracket is a flat profile: outline, mounting holes, lightening slots and any half-etched weight pockets, all cut in one pass. What etching cannot do is bend it — a bracket that leaves the line with a fold in it is a formed part, and forming is an outsourced step here, not an in-house one. Say so on the enquiry if the design needs a bend, and the quotation will show it as a separate step. The TMNetch guide draws the same line from the other side: chemical etching suits thin titanium parts with fine openings and complex geometries; CNC machining is usually better for thick or three-dimensional features. A 3 mm bracket with a deep pocket is a machining job, not an etching job — and a supplier who says otherwise is selling the process, not the part.
Weight, worked as arithmetic
Weight saving from titanium is not a performance claim; it is density times volume. Titanium at ≈ 4.5 g/cm³ against steel at ≈ 7.9 g/cm³ means the same outline at the same thickness weighs about 57% of the steel part — a saving of a little over 40% per part. Across a shim set or a run of brackets, that is the number to put in the trade-off table, next to the cost of the material and the cost of the process. Grade choice moves the other side of the table: Grade 2 (commercially pure, ≥ 99.2% Ti per ASTM B265, tensile strength ≥ 345 MPa) is the corrosion-first choice; Grade 5 (Ti-6Al-4V) is the strength-first alloy for brackets that carry load. Do not specify Grade 5 where Grade 2 will do — the alloy costs more and etches no faster — and do not specify Grade 2 where the bracket is structural. The grade belongs on the drawing, with the thickness, not in the email thread.
Half-etching is the second weight lever, and it is an etching-only one: a pocket etched 50–75% through the sheet, depth controlled to ±0.05 mm, removes material where the bracket does not need it while leaving the full thickness where it does — around a mounting hole, along a stiffening rib line. A stamped or machined pocket needs a second operation; an etched pocket is part of the same pass. The limit is the same as ever: the remaining web must stay flat and the pocket floor must stay within its depth tolerance, so deep narrow pockets on thin stock are the wrong shape to ask for.
The four drawing items
- Material and grade. State titanium, and the grade — Grade 2 or Grade 5 — with the reason in one line (corrosion exposure, or structural load). If the media or the environment points elsewhere, say so: we etch stainless steel, copper, brass and nickel as well, and the honest answer is sometimes a different metal. Our buying guide walks through the same four items for any etched part.
- Thickness. This is the functional dimension for a shim and the weight dimension for a bracket. Put the nominal thickness and design around ±10% of it. Do not specify below our stocked 0.05 mm, and do not specify a tolerance tighter than ±10% without asking first — a shim specified at ±0.005 mm on 0.1 mm stock is asking for a tolerance the process does not hold.
- Feature sizes. Any through-feature — mounting hole, slot, lightening cutout — follows the thickness rule: roughly 0.8–1.2× the material thickness as a minimum. A 0.20 mm hole in 0.3 mm stock is a declined enquiry; the fixes are thinner stock or a larger feature. Half-etched pockets run 50–75% of thickness with ±0.05 mm depth control. Put the minimum feature on the drawing next to the thickness, so the feasibility check is visible before the quote.
- Finish and edge. State the finish — passivation is available in-house; plating and other surface treatment are outsourced — and state the edge condition if it matters (burr-free is the etched default). If the bracket needs a bend, state the bend as a separate forming step so it is quoted, not assumed. The passivation and plating post sets out what to specify on the drawing for finishes.
What etching does — and what it does not do
Photo-chemical etching removes metal chemically, not mechanically, so a thin titanium shim or bracket comes out flat, stress-free and burr-free, with the same artwork producing the first article and the ten-thousandth. That repeatability is the case for etching aircraft shims: a tolerance stack that depends on shim thickness cannot absorb a supplier whose thickness wanders. The same discipline behind etched flow fields — channel depth, pitch and flatness — is set out in our bipolar-plate post for PEM electrolyzers, a different product but the same etched-channel logic.
The boundaries are equally plain. Etching makes flat parts — sheets up to 600 × 1,450 mm at 0.5 mm and above — not coil or reel-fed strip, not deep-drawn housings, not thick machined brackets. We do not etch aluminium, we do not apply fuel-cell coatings, and we do not build brazed or diffusion-bonded assemblies. Fotofab’s AS9100D, ISO 9001 and ITAR status is that company’s certification, not ours; our quality documentation is PPAP Level 3, material test certificates and per-run batch numbers. An aircraft buyer who needs a certified aerospace quality system should ask for our current quality documentation at quotation and judge it on its own terms.
FAQ
Why etch a titanium shim instead of stamping it? Stamping is fast and cheap at volume, but it stresses thin sheet, leaves a burr and a break edge, and needs a die for every revision. Etching cuts chemically — no stress, no burr, no heat-affected zone — and a revision is new artwork. For thin shims, tight thickness tolerance and frequent revision, etching is the better process; for thick, simple, high-volume blanks, stamping may win.
How thin can an aircraft shim be? Our stocked gauges start at 0.05 mm. Tolerance is ±10% of thickness at any gauge — ±0.005 mm on 0.05 mm stock, ±0.01 mm on 0.1 mm stock, ±0.02 mm on 0.2 mm stock. Below 0.05 mm, ask first; the gauge may need to be sourced per order.
Can you etch the mounting holes and lightening slots in the same part? Yes, where they fit the thickness rule (roughly 0.8–1.2× the material thickness). A 0.20 mm hole in 0.3 mm stock is a declined enquiry; the fixes are thinner stock or a larger feature. Half-etched weight pockets are available at 50–75% of thickness with ±0.05 mm depth control.
Grade 2 or Grade 5 for a bracket? Grade 2 for corrosion exposure and non-structural brackets; Grade 5 (Ti-6Al-4V) where the bracket carries load. State the grade and the reason on the drawing. Do not specify Grade 5 by default — it costs more and etches no faster.
Can the bracket be bent after etching? A bend is a forming step, and forming is outsourced here, not in-house. State the bend on the enquiry so it is quoted as a separate step, with its own tolerance. A flat etched profile with no bend is the straightforward etched part.
What do you need to quote a titanium shim or bracket? The four drawing items in this post: material and grade, thickness, feature sizes, and finish/edge — plus the bend, if any. Samples take 3–5 days when the material is in stock, production 7–10 days, no minimum order quantity, US$100 minimum order charge, FOB.
This post was written by Xinketching — a precision photo-etching manufacturer in Dongguan, China, producing flat etched metal parts since 2005. If you are specifying a titanium shim or bracket for an aircraft assembly, send the drawing and we will quote the etched part.
- What Does a 770 W/cm² GPU Hotspot Mean for the Etched Copper Flow Layer? - November 22, 2026
- Photo-Etched Precision Medical Metal Components: Micro-Needles, Lancets and Microfluidic Parts - November 21, 2026